WC-10Co4Cr Carbides poda kwa mashine ya jumla
Maelezo
KF-65 ni poda ya ubora wa juu ya WC-10Co4Cr ambayo imeundwa kukidhi mahitaji ya juu ya sekta ya petroli, karatasi, na mashine za jumla.Bidhaa hii ina ukubwa mbalimbali wa chembe 15-45/ 10-38/ 5-30/ 5-15/ 5-25μm, na kuifanya kufaa kwa matumizi mbalimbali.
KF-65 inapatikana katika aina mbili tofauti: sinter & crush, na agglomerated & sintered.Sinter & sintered fomu hutengenezwa kwa kunyunyiza poda na kisha kukandamizwa katika vipande vidogo, wakati fomu iliyounganishwa na sintered inafanywa kwa kuunganisha unga ndani ya chembe kubwa zaidi kabla ya kuoka.Utangamano huu hurahisisha kujumuisha KF-65 katika mchakato wako wa utengenezaji na kufikia matokeo unayotaka.
Zaidi ya hayo, KF-65 inaweza kulinganishwa na bidhaa zingine zinazoongoza kama vile AMPERIT 554/556/557/558, METCO/AMDRY 5843/5163, WOKA 3903/3615/3652/3655/3665, PRAXAIR WC-1316-WC-116-WC-113/WC /WC-7311350, na PAC 1500. Hii inahakikisha kuwa unapokea bidhaa ya ubora wa juu inayofikia viwango sawa na chapa zingine zinazoongoza katika tasnia.
Mojawapo ya faida kuu za KF-65 ni uwezo wake wa kutumika kama mbadala wa uwekaji wa chromium ngumu.Hili ni jambo la kuzingatia kwa makampuni yanayotaka kupunguza athari zao za kimazingira na kuzingatia kanuni.Zaidi ya hayo, KF-65 inaweza kutoa uso laini kumaliza, kupunguza au hata kuondoa haja ya baada ya machining.Hii inaweza kuokoa muda na pesa katika mchakato wa utengenezaji, wakati bado ikitoa matokeo ya ubora wa juu.
Iwe unatazamia kuboresha utendakazi wa kifaa chako, kupunguza athari zako kwa mazingira, au kuboresha tu ubora wa bidhaa zako, KF-65 ni chaguo bora.Ni suluhisho la kuaminika na la gharama nafuu ambalo linaweza kukidhi mahitaji ya aina mbalimbali za viwanda, ikiwa ni pamoja na mafuta ya petroli, karatasi, na mashine za jumla.Ijaribu leo na ujionee tofauti hiyo.
Bidhaa zinazofanana
Chapa | Jina la bidhaa | AMPERIT | METCO/AMDRY | WOKA | PRAXAIR | PAC |
KF-65 | WC-10Co4Cr | 554 | 5843 | 3903 | WC-113WC-436-1 | |
WC-10Co4Cr | 556 / 557 / 558 | 5163 | 3651 / 36523655 / 3665 | WC-7311350 | 1500 | |
WC-10Co4Cr | . | . | 3660FC | . | 1500 |
Vipimo
Chapa | Jina la bidhaa | Ukubwa wa Chembe (μm) | Kemia (wt%) | Aina | Msongamano unaoonekana | Uwezo wa kubadilika | Mali | Maombi | |||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Co | C | Fe | W | Cr | B | Si | Ni | ||||||||
KF-65 | WC-10Co4Cr | 15-45, 10-38 | 9.5-10 | 5.3-5.6 | ≤0.8 | Bal. | 3.5-4.0 | Sinter&Crush | 5.5-6.5g/cm3 | ≤25 s/50g | APS,HVOF,HVAF | Mchoro mbadala wa chromium ngumu;Petroli, karatasi, mashine ya jumla | |||
KF-65 | WC-10Co4Cr | 15-45,10-38,5-30 | 9.5-10 | 5.3-5.6 | ≤0.8 | Bal. | 3.5-4.0 | Agglomerated na sintered | 4.0-6.0 g/cm3 | ≤18 s/50g | APS,HVOF,HVAF | Mchoro mbadala wa chromium ngumu;Petroli, karatasi, mashine ya jumla | |||
KF-65 | WC-10Co4Cr | 5-25,5-15 | 9.5-10 | 5.3-5.6 | ≤0.8 | Bal. | 3.5-4.0 | Agglomerated na sintered | 3.5-4.8 g/cm3 | Kulisha kwa utulivu kwa kulisha poda | HVOF,HVAF | Uwekaji mbadala wa chromium ngumu; Uso laini, uchakataji wa machapisho kidogo au bila malipo; | |||
KF-60 | WC-12Co | 15-45, 10-63 | 10.5-12 | 4.9-5.4 | ≤0.8 | Bal. | Sinter&Crush | 5.5-6.5 g/cm3 | ≤25 s/50g | APS, HVOF | Kuvaa upinzani,Fretting kuvaa upinzani | ||||
KF-60 | WC-12Co | 15-45, 10-38, 5-30 | 10.5-12 | 4.9-5.4 | ≤0.8 | Bal. | Agglomerated na sintered | 4.0-6.0 g/cm3 | ≤18 s/50g | APS,HVOF,HVAF | Kuvaa upinzani,Fretting kuvaa upinzani; mashine ujumla | ||||
KF-61 | WC-17Co | 15-45, 10-38 | 15.5-17 | 4.5-5.1 | ≤0.8 | Bal. | Agglomerated na sintered | 3.5-5.5 g/cm3 | ≤25 s/50g | APS,HVOF,HVAF | Kuvaa upinzani,Fretting kuvaa upinzani,Bora ushupavu; ujumla mashine | ||||
KF-62 | WC-25Co | 15-45, 10-38 | 22-26 | 4.0-4.6 | ≤0.8 | Bal. | Agglomerated na sintered, Densification | 3.0-5.5 g/cm3 | ≤25 s/50g | APS, bunduki za mlipuko, dawa ya baridi | Fretting kuvaa upinzani,Bora ushupavu | ||||
KF-66 | WC-23%CrC-7Ni | 15-45, 10-38 | 6.0-6.8 | ≤0.8 | Bal. | 16.5-20 | 5.5-7 | Agglomerated na sintered | 3.0-5.0 g/cm3 | ≤25 s/50g | APS,HVOF,HVAF | Upako mbadala wa chromium ngumu; Hutumika kwa mazingira ya asidi/alkali ya ukolezi wa chini ifikapo 200 ℃;Kinga oxidation na upinzani kuvaa ifikapo 750 ℃ | |||
KF-66 | 43WC-43%CrC-14Ni | 15-45,10-38 | 7.8-8.4 | ≤0.8 | Bal. | 35-38 | 12-14 | Agglomerated na sintered | 2.0-4.0 g/cm3 | ≤35 s/50g | APS,HVOF,HVAF | Uwekaji mbadala wa chromium ngumu Hutumika kwa mazingira ya asidi/alkali ya ukolezi mdogo ifikapo 200 ℃ | |||
KF-63 | WC-10Ni | 15-45,10-38 | 4.5-5.2 | ≤0.1 | Bal. | 8.5-10.5 | Agglomerated na sintered | 4.0-6.0 g/cm3 | ≤18 s/50g | APS, HVF, HVAF | Mipako isiyo na sugu ya kuvaa sumaku.Upinzani bora wa kutu | ||||
KF-70 | Cr3C2-25NiCr | 15-45, 20-53 | 9-11 | ≤1 | Bal. | 18-21.5 | Agglomerated na sintered | ≥2.3 g/cm3 | Kulisha kwa utulivu kwa kulisha poda | APS, HVOF | Kinga oxidation na upinzani kuvaa ifikapo 815 ℃ | ||||
KF-69 | Cr3C2-20NiCr | 15-45, 20-53 | 9-11 | ≤1 | Bal. | 15-17.5 | Agglomerated na sintered | ≥2.3 g/cm3 | Kulisha kwa utulivu kwa kulisha poda | APS, HVOF | Kinga oxidation na upinzani kuvaa ifikapo 815 ℃ | ||||
KF-71 | Cr3C2-30NiCr | 15-45, 20-53 | 9-11 | ≤1 | Bal. | 15-17.5 | Agglomerated na sintered | ≥2.3 g/cm3 | Kulisha kwa utulivu kwa kulisha poda | APS, HVOF | Kinga oxidation na upinzani kuvaa ifikapo 815 ℃.Ushupavu bora | ||||
KF-60 | WC-12Co (Kaboni Chini) | 15-45, 20-53 | 10.5-12 | 4.0-4.4 | ≤0.8 | Bal. | Agglomerated na sintered | 4.0-6.0 g/cm3 | ≤18 s/50g | HVOF,HVAF | Inatumika kwa safu za umwagaji wa Zn katika Mistari inayoendelea ya Mabati | ||||
KF-68 | WC-30WB-10Co | 15-45,20-53,10-38 | 9-11 | 3.5-3.9 | Bal. | 1.4-1.7 | Agglomerated na sintered | 3.0-4.9 g/cm3 | ≤30 s/50g | HVOF,HVAF | Inatumika kwa safu za umwagaji wa Zn katika Mistari inayoendelea ya Mabati | ||||
KF-68 | WC-30WB-5Co5Cr | 15-45,20-53,10-38 | 4-6 | 3.5-3.9 | Bal. | 4-6 | 1.4-1.7 | Agglomerated na sintered | 3.0-4.9 g/cm3 | ≤30 s/50g | HVOF,HVAF | Inatumika kwa safu za umwagaji wa Zn katika Mistari inayoendelea ya Mabati | |||
KF-300E | 35%WC-NiCrBSi | 15-53,45-104 | 2.5-3.2 | 1.0-2.6 | 32-35 | 7.5-9 | 1.5-1.9 | 2.0-2.7 | Bal. | WC na aloi ya kutengeneza NiCrBSi | 4.0-4.9 g/cm3 | ≤16 s/50g | HVOF, PS | Aina Mbadala Iliyochanganywa WC+Ni60;Matumizi ya nyenzo ya juu,Matumizi ya chini ya nishati, athari ya chini ya mafuta;Hutumika kwa ukungu wa glasi | |
KF-300F | 50%WC-NiCrBSi | 15-53,45-104 | 3.2-4.3 | 0.8-2.0 | 45-48 | 5.8-7.2 | 1.0-1.7 | 1.5-2.4 | Bal. | WC na aloi ya kutengeneza NiCrBSi | 5.0-7 g/cm3 | ≤16 s/50g | HVOF, PS | Aina Mbadala Iliyochanganywa WC+Ni60;Matumizi ya nyenzo ya juu,Matumizi ya chini ya nishati, athari ya chini ya mafuta;Hutumika kwa ukungu wa glasi |